major elements [wt %]
CRB | RV | 1sRV | Z-Score | |
Na₂O | < 0,070 | 0,101 | 0,066 | --- |
MgO | 1,550 | 1,576 | 0,213 | -0,100 |
Al₂O₃ | 71,470 | 71,230 | 0,855 | 0,200 |
Cr₂O₃ | 0,117 | 0,109 | 0,016 | 0,400 |
P₂O5 | 0,037 | 0,026 | 0,010 | 0,900 |
K₂O | 0,165 | 0,177 | 0,020 | -0,500 |
CaO | 1,420 | 1,376 | 0,076 | 0,400 |
TiO₂ | 1,353 | 1,270 | 0,175 | 0,400 |
Fe₂O₃ tot | 1,300 | 1,412 | 0,140 | -0,700 |
LOI | 1,190 | 1,340 | 0,250 | -0,500 |
C-frei | 0,900 | 1,060 | 0,227 | -0,600 |
C-gesamt | 2,830 | 2,310 | 0,070 | 6,500 |
Si-gesamt | 11,630 | 11,720 | 0,510 | -0,200 |
SiC | 6,400 | 3,870 | 0,722 | 2,900 |
SiO₂ | 15,260 | 14,760 | 0,503 | 0,300 |
trace elements [µg/g]
CRB | RV | 1sRV | Z-Score | |
Mn₂O₃ | 0,057 | 0,049 | 0,018 | 0,40 |
ZrO₂ | 0,107 | 0,099 | 0,016 | 0,40 |
Legend