RFA, XRF, Röntgenfluoreszensanalyse RFA Ringversuch IRMA - GSMS-3, marines Sediment
Veranstalter des Ringversuchs:
Institute of Rock and Mineral Analysis (IRMA) of the Chinese Academy of Geological Sciences
Ringversuchsmaterial:
GSMS-3 (marines Sediment)
RV geschlossen:
1995 - 11
Literatur:
GEOSTANDARDS NEWSLETTERS, Vol. 19, No. 2, 1995, GEOSTANDARDS NEWSLETTERS, Vol. 22, No. 1, 1998
Hauptelemente [MA%]
CRB | RV | 1sRV | Z-Score | |
Na₂O | 3,850 | 3,750 | 0,144 | |
MgO | 2,030 | 2,040 | 0,080 | |
Al₂O₃ | 7,880 | 7,750 | 0,343 | |
SiO₂ | 31,620 | 31,630 | 0,524 | |
P₂O5 | 0,328 | 0,330 | 0,015 | |
SO₃ | 0,698 | 0,510 | 0,200 | |
K₂O | 1,600 | 1,600 | 0,132 | |
CaO | 22,860 | 22,400 | 1,032 | |
TiO₂ | 0,390 | 0,380 | 0,032 | |
Fe₂O₃ tot | 3,930 | 3,790 | 0,153 | |
MnO | 0,408 | 0,400 | 0,016 |
Spurenelemente [µg/g]
CRB | RV | 1sRV | Z-Score | |
As | 7,00 | 5,00 | 1,23 | |
Ba | 2630,00 | 2500,00 | 230,00 | |
Ce | 54,00 | 54,30 | 4,20 | |
Cl | 21100,00 | 32700,00 | 563,00 | |
Co | 52,00 | 53,40 | 4,20 | |
Cr | 44,00 | 35,40 | 8,50 | |
Cu | 248,00 | 232,00 | 9,60 | |
F | 1226,00 | 700,00 | 110,00 | |
Ga | 11,00 | 11,40 | 0,70 | |
Hf | 2,00 | 2,40 | 0,34 | |
La | 67,00 | 44,10 | 3,70 | |
Mo | 5,00 | 6,00 | 1,10 | |
Nb | 11,00 | 7,20 | 1,00 | |
Ni | 105,00 | 107,00 | 11,50 | |
Pb | 25,00 | 22,00 | 5,20 | |
Rb | 46,00 | 49,80 | 4,80 | |
Sr | 618,00 | 668,00 | 72,00 | |
Th | 7,60 | 7,10 | 0,60 | |
U | 2,10 | 1,10 | 0,30 | |
V | 68,00 | 68,60 | 5,80 | |
Y | 65,00 | 69,30 | 7,30 | |
Zn | 139,00 | 140,00 | 24,50 | |
Zr | 97,00 | 96,00 | 4,80 |
Legende
CRB
Ergebnisse CRB
Ringversuch
Ergebnisse Ringversuch
1s-RV
Standardabweichung Ringversuch
Z-Score
Differenz des Messwerts vom Mittelwert des Ringversuchs
*
Wert nicht zertifiziert